Solvay Chemicals Grade A Barium Hydroxide Octahydrate

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Grade A Barium Hydroxide Octahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Solvay
Processing Properties Metric English Comments
Moisture Content 2.0 %
2.0 %
Descriptive Properties Value Comments
Appearance wet product
Composition 8 ppm
Fe
Users viewing this material also viewed the following: