Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride >94%

Category Ceramic , Halide
Manufacturer Solvay Chemicals
Trade Name CASO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride >94%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2 Applications: Food processing aid, agriculture, chemical industry, oil industry, winter road, environment, industrial and domestic drying and dust controlInformation provided by Solvay
Physical Properties Metric English Comments
Density <= 0.700 g/cc

@Temperature 0.850 °C
<= 0.0253 lb/in³

@Temperature 33.5 °F
Molecular Weight 111 g/mol
111 g/mol
Descriptive Properties Value Comments
Appearance White granules
Composition <0.004%
Fluorides
<0.01 mg/kg
Hg
<3.0 mg/kg
As
>940 g/kg
CaCl2, Specifications
0.016 mg/kg
Acid insoluble matter
0.3 g/kg
SO4
0.4 g/kg
MgCl2
0.4 mg/kg
Pb
0.5 g/kg
Water insoluble matter
0.5 g/kg
Ca(OH)2
3.7 g/kg
Fe
32 g/kg
Magnesium & alkali salts
33 g/kg
NaCl
953 g/kg
CaCl2
Granulometry 0.11
<1.25 mm
0.58
<2.0 mm
0.83
<2.8 mm
0.96
<5.0 mm