Solvay Chemicals Blanc fixe N

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Blanc fixe N.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blanc Fixe N is the optimal extender for almost all applications in the production of paints and coatings and plastic. Furthermore, it is used as a chemical in lead acid batteries.Information provided by Solvay
Physical Properties Metric English Comments
Particle Size 1.7 µm
1.7 µm
Descriptive Properties Value Comments
Conductivity 100 µS/cm
Oil Index 13 g/100g