Material Notes:
Chloroform is a non-flammable product.EINECS Number: 200-663-8/CAS Number: 67-66-3/UN number: 1888Information provided by Solvay
Physical Properties Metric English Comments
Density 1.478 - 1.492 g/cc
0.05340 - 0.05390 lb/in³
1.415 g/cc

@Temperature 60.0 °C
0.05112 lb/in³

@Temperature 140 °F
1.434 g/cc

@Temperature 50.0 °C
0.05181 lb/in³

@Temperature 122 °F
1.452 g/cc

@Temperature 40.0 °C
0.05246 lb/in³

@Temperature 104 °F
1.461 g/cc

@Temperature 35.0 °C
0.05278 lb/in³

@Temperature 95.0 °F
1.471 g/cc

@Temperature 30.0 °C
0.05314 lb/in³

@Temperature 86.0 °F
1.48 g/cc

@Temperature 25.0 °C
0.0535 lb/in³

@Temperature 77.0 °F
1.489 g/cc

@Temperature 20.0 °C
0.05379 lb/in³

@Temperature 68.0 °F
1.498 g/cc

@Temperature 15.0 °C
0.05412 lb/in³

@Temperature 59.0 °F
1.508 g/cc

@Temperature 10.0 °C
0.05448 lb/in³

@Temperature 50.0 °F
1.517 g/cc

@Temperature 5.00 °C
0.05481 lb/in³

@Temperature 41.0 °F
1.526 g/cc

@Temperature 0.000 °C
0.05513 lb/in³

@Temperature 32.0 °F
Viscosity 0.40 cP

@Temperature 60.0 °C
0.40 cP

@Temperature 140 °F
Dynamic
0.43 cP

@Temperature 50.0 °C
0.43 cP

@Temperature 122 °F
Dynamic
0.47 cP

@Temperature 40.0 °C
0.47 cP

@Temperature 104 °F
Dynamic
0.49 cP

@Temperature 35.0 °C
0.49 cP

@Temperature 95.0 °F
Dynamic
0.51 cP

@Temperature 30.0 °C
0.51 cP

@Temperature 86.0 °F
Dynamic
0.54 cP

@Temperature 25.0 °C
0.54 cP

@Temperature 77.0 °F
Dynamic
0.57 cP

@Temperature 20.0 °C
0.57 cP

@Temperature 68.0 °F
Dynamic
0.60 cP

@Temperature 15.0 °C
0.60 cP

@Temperature 59.0 °F
Dynamic
0.63 cP

@Temperature 10.0 °C
0.63 cP

@Temperature 50.0 °F
Dynamic
0.67 cP

@Temperature 5.00 °C
0.67 cP

@Temperature 41.0 °F
Dynamic
0.71 cP

@Temperature 0.000 °C
0.71 cP

@Temperature 32.0 °F
Dynamic
Molecular Weight 119.4 g/mol
119.4 g/mol
Vapor Pressure 0.0780 bar

@Temperature 0.000 °C
58.5 torr

@Temperature 32.0 °F
0.101 bar

@Temperature 5.00 °C
75.8 torr

@Temperature 41.0 °F
0.130 bar

@Temperature 10.0 °C
97.5 torr

@Temperature 50.0 °F
0.165 bar

@Temperature 15.0 °C
124 torr

@Temperature 59.0 °F
0.207 bar

@Temperature 20.0 °C
155 torr

@Temperature 68.0 °F
0.258 bar

@Temperature 25.0 °C
194 torr

@Temperature 77.0 °F
0.318 bar

@Temperature 30.0 °C
239 torr

@Temperature 86.0 °F
0.390 bar

@Temperature 35.0 °C
293 torr

@Temperature 95.0 °F
0.475 bar

@Temperature 40.0 °C
356 torr

@Temperature 104 °F
0.689 bar

@Temperature 50.0 °C
517 torr

@Temperature 122 °F
0.974 bar

@Temperature 60.0 °C
731 torr

@Temperature 140 °F
Descriptive Properties Value Comments
Appearance Clear without suspended matter
ASTM D3741/B
Color <10
APHA
Composition <1 mg/kg
Oxidizing Compounds (Cl2)
<5 mg/kg
Acidity (HCl)
<50 mg/kg
Moisture (H2O)
Purity >999 g/kg
without Stabilizers
Residue on Evaporation <10 mg/kg