Material Notes:
Description: Aluminum Sulfate, Solution, technical grade is a clear, water white to slightly yellow-brown liquid. It complies with the standards of the American Water Works Association B403-98. It has been certified by the National Sanitation Foundation (NSF) for use in the treatment of drinking water at a maximum dosage of 150 mg/L (dry basis). Formula: Al2(SO4)3 (In aqueous solution Nomenclature: Aluminum Sulfate, Solution Liquid AlumCAS: 10043-01-3CAS Index: Sulfuric Acid, Aluminum Salt (3:2)Available in: North AmericaUses: Chemical: In leather tanning, fur dressing, and catalyst manufacturing; Pulp and Paper: In the manufacture of paper; Textiles: As a mordant in dyeing; and Water Treatment: The treatment of water and waste water in coagulation, flocculation and phosphorous removalInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.33 g/cc

@Temperature 60.0 °C
0.0480 lb/in³

@Temperature 140 °F
For 8.25% Al<sub>2</sub>O<sub>3</sub> solution
pH 0.20 - 2.5
0.20 - 2.5
acidic to basic, For 8.25% Al<sub>2</sub>O<sub>3</sub> solution
2.2 - 4.0
2.2 - 4.0
1% solution, acidic to basic, For 8.25% Al<sub>2</sub>O<sub>3</sub> solution
Molecular Weight 342.2 g/mol
342.2 g/mol
Thermal Properties Metric English Comments
Melting Point -15.5 °C
4.10 °F
Freezing Point
Descriptive Properties Value Comments
Assay >26.9%
As Aluminum Sulfate, Anhydrous Al<sub>2</sub>(SO<sub>4</sub>)<sub>3</sub>
>8.0%
As available Water Soluble Al<sub>2</sub>O<sub>3</sub>
Copyright © lookpolymers.com All Rights Reserved