Material Notes:
Description: Linear Alcohol EO/PO.Identification: ETHO-PROPOXYLATED FATTY ALCOHOLCAS: 68603 - 25 – 8Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Wetting agent, water soluble and oil dispersible surfactant.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
pH 6.0 - 7.0
6.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 5.00 °C
41.0 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Refractive Index 1.441

@Temperature 60.0 °C
1.441

@Temperature 140 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Liquid
Cloud Point 50-60°C
1.0% in water, RPG08
Composition Active
1
Ionic Charge Nonionic
Users viewing this material also viewed the following: