Material Notes:
Description: Branched alcohol EO/PO. Excellent hard surface cleaning with controlled foam. Very free rinsing.Chemical Name: BRANCHED ALCOHOL EO/POCAS: 37251-67-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX© LA-EP-16 is a branched alcohol EO/PO. Excellent hard surface cleaning with controlled foam. Very free rinsing. Automatic-Dish Washing Detergents, Hard Surface Cleaners, Miscellaneous Cleaners, Vehicle CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
10% Solution; RP-0420
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
RP-0064
Cloud Point 59-61°C
1.0% Solution, RP-0124