Solvay ANTAROX® FM 63 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ANTAROX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ANTAROX® FM 63 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Linear Alcohol EO/POIdentification: ETHOPROPOXYLATED FATTY ALCOHOLCAS: 68154 – 97 – 2Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Fabric and Home Care: Low foam. Wetting agent. Industrial formulations: Low-foaming detergent and wetting agent for liquid detergent formulations and cutting oils. Metal treatment: Low-foaming detergent and wetting agent for liquid detergent formulations and cutting oils.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
pH 6.0 - 7.5
6.0 - 7.5
1% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.60 %
<= 0.60 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Liquid
Cloud Point 43-47°C
0.5% in water, RPG08
Composition Active
1
Ionic Charge Nonionic