Material Notes:
Description: Antarox BL-725 is an effective wetting agent for rinse aids and detergent applications. Antarox BL-725 is also used in textile and metal treatment applications.Chemical Name: DETERGENT RANGE ALCOHOL ALKOXYLATECAS: 68551-13-3 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX® BL-725 is an effective wetting agent for rinse aids and detergent applications. ANTAROX® BL-725 is also used in textile and metal treatment applications. Automatic-Dish Washing Detergents, Laundry Detergent Liquids, Laundry Detergent Powders and Tablets, Miscellaneous CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
pH 5.0 - 8.0
5.0 - 8.0
5% Solution; RP-0420
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clean, Clear Liquid
RP-0064
Composition Active
>90%