Solvay ANTAROX® BL 330 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ANTAROX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ANTAROX® BL 330 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Biodegradable Chlorine capped non-ionic, low-foaming characteristics, excellent surface-active properties as well as acid and alkali stability. Effective de-dusting agent for powdered detergents. Also used in rinse aids, bottle cleaning, dairy cleaners and steam systems, food plant cleaning and mechanical dish wash powders. Compliant with the EU's detergent biodegradability regulation.Identification: Linear alcohol E/O-Chlorine CappedCAS: 69227-21-0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX BL-330 is a detergent, wetting agent for rinse aids and defoaming agent for metal cleaning and industrial cleaners.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
RP-0138
Processing Properties Metric English Comments
Moisture Content 3.0 - 6.0 %
3.0 - 6.0 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Fluid Liquid
RP-0064
Cloud Point 38-33°C
10% Solution, RP-0124
Users viewing this material also viewed the following: