Solvay ALKAMULS® S 80 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® S 80 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: SORBITAN MONOOLEATECAS: 1338 - 43 – 8EINECS: 215 – 665 – 4Available in: Asia Pacific, Europe, Latin America and North America. Solubility: Dispersible in water. Soluble in most polar and aromatic solvents. Applications: Recommended emulsifier for inverse water/oil emulsions. Used to formulate industrial emulsion in polyacrylamide production and explosive emulsionsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.970 - 0.980 g/cc
0.0350 - 0.0354 lb/in³
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 9.0
<= 9.0
OA-71_1
Chemical Properties Metric English Comments
Total Acid Number <= 8.0
<= 8.0
[mg KOH/g]; ISO 660
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
NF T 20052
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Liquid
OS-500
Composition Active
1
HLB number 4.3
Hydroxyl Number 190-210 mg KOH/g
OA-086
Ionic Charge Nonionic
Peroxide value <3 meq/kg
NF T 60 220
Saponification number 150-160 mg KOH/g
OA-507