Solvay ALKAMULS® OR 36 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® OR 36 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ethoxylated castor oil. Emulsifier for oil and waxes in water based formulations. Used as dispersant for pigments and iron powders. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling agent. Softening and rewetting agent for wet strength paper. Stabilizer for PVAc emulsion paints. Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 13.Identification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifier for Agrochemical formulations. Industrial formulations/Metal treatment : Emulsifier for oil and waxes in water based formulations. Used as dispersant for pigments and iron powders. Emulsifier for fats, oils, fatty acids, waxes and solvents. Dispersant for pigments and iron powders in magnetic coupling fluids. Paper dye-leveling agent. Softening and rewetting agent for wet strength paper. Stabilizer for PVAC emulsion paints. Emulsifier for Home and Personal Care formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc

@Temperature 50.0 °C
0.0376 lb/in³

@Temperature 122 °F
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 12.0 °C
53.6 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous Liquid
Composition Active content
1
HLB number 13.1
Ionic Charge Nonionic
Saponification number 60-69 mg KOH/g
RPG05