Material Notes:
Description: Emulsifying agent for agrochemical formulationsIdentification: BLEND OF FATTY ACIDSSolubility: Insoluble in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifying agent for agrochemical formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
Thermal Properties Metric English Comments
Pour Point 6.00 °C
42.8 °F
Flash Point >= 180 °C
>= 356 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Composition Active content
1
Ionic Charge Anionic
Saponification number 199-205 mg KOH/g
RPG05