SolVin 460SL Polyvinyl Chloride grafted copolymer

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer SolVin
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SolVin 460SL Polyvinyl Chloride grafted copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made by suspension polymerization. Special product for calendered film from the high temperature process. APPLICATIONS Calendering : unplasticized PVC - film : high temperature process Extrusion : unplasticized PVC - sheet, filmInformation provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ISO 60
Particle Size 63 µm
63 µm
>90% greater than value; ISO 1624
250 µm
250 µm
<2% greater than value; ISO 1624
Viscosity Test 87 cm³/g
87 cm³/g
Reduced viscosity, K value = 59.5; ISO 1628-2