Sinotek Materials Packing Expanded Graphite Yarns

Category Carbon , Graphite
Manufacturer Sinotek Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sinotek Materials Packing Expanded Graphite Yarns.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Expanded graphite yarns are made of twists of low-sulphur expanded combined with reinforcing materials, and are suitable for weaving of expanded graphite braided packings. There is a wide variety of reinforcing materials used in the yarn twisting of different working conditions, with include cotton yarn, fiberglass, carbonized fiber, wires of nickel alloy or stainless steel or copper.Information provided by Sinotek