Sinotek Materials Graphite Sealing Strip Fireproofing Sealing Products

Category Carbon , Graphite
Manufacturer Sinotek Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sinotek Materials Graphite Sealing Strip Fireproofing Sealing Products.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The graphite sealing strip is made from a graphite based mineral fiber with stabilized high density, which is designed to activate (expand) at 180° with an expansion ratio of 35:1. The intumescent strip around the door expands at high temperatures to seal housing and provide a ‘flame break’. It can adhibit on windowsills, door-apertures, and all kinds of pipe-line apertures, etc. When fire or high temperature occurs, and expand temperature is achieved, it can expand and block the aperture completely. This materials usually is used on buildings. Information provided by Sinotek
Descriptive Properties Value Comments
Expansion Ratio, % 3500