Silberline Tufflake® 3720

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Tufflake®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Tufflake® 3720.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating applications and metallic finishes.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
Bulk Factor 0.069
0.069
Volatiles 24 %
24 %
Particle Size 16 µm
16 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.01% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash