Silberline Sparkle Silver® 5245-AR

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® 5245-AR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silver® 5245-AR is a medium, non-leafing aluminum pigment. It provides a bright, white, clean face tone with exceptionally dark flop effect. It has narrow particle size distribution. Close packing in basecoat films ensures maximum distinctiveness of image (D.O.I.).Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Bulk Factor 0.083
0.083
Volatiles 38 %
38 %
Particle Size 21 µm
21 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.01% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash