Silberline Sparkle Silver® 3333-AR

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® 3333-AR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silver® 3333-AR is an acid resistant pigment developed for formulators requiring good face whiteness, with a fine appearance. Close packing and good distinctiveness of image (D.O.I.) make Sparkle Silver® 3333-AR a good choice for basecoat/clear automotive systems.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
Bulk Factor 0.087
0.087
Volatiles 40 %
40 %
Particle Size 15 µm
15 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash