Silberline Sparkle Silver® 3141-ST

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® 3141-ST.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silver® 3141-ST is a coarse high sparkle, non-leafing aluminum pigment popular for Automotive Applications. This pigment can be used with tints to produce a wide range of polychromatic effects.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
Bulk Factor 0.080
0.080
Volatiles 34 %
34 %
Particle Size 30 µm
30 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash