Silberline Sparkle Silver® 3122-AR

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® 3122-AR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silver® 3122-AR is a coarse, non-leafing, acid stain resistant aluminum flake pigment. It is characterized by high sparkle, a white face color and deep flop. The main applications are high quality industrial finishes and bicycle and automotive component paints. A regular purity version, Sparkle Silver® 3622, is also available.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.79 g/cc
1.79 g/cc
Bulk Factor 0.066
0.066
Volatiles 22 %
22 %
Particle Size 36 µm
36 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash