Silberline Glamour Flake® 058-PA

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Glamour Flake®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Glamour Flake® 058-PA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glamour Flake 058-PA is a coarse round flake with a high sparkle, brilliant appearance. This pigment can be used with tints to produce a wide range of polychromatic effects.Applications: Cosmetics
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
Volatiles 30 %
30 %
Descriptive Properties Value Comments
Solvents Isopropyl Alcohol