Material Notes:
SBR-1500. For use in the shoe industry and for production of vulcanized micro-porous sole rubbers and rubber technical articles.
Physical Properties Metric English Comments
Mooney Viscosity 45 - 57

@Temperature 100 °C
45 - 57

@Temperature 212 °F
ML 1-4
Ash <= 0.60 %
<= 0.60 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 26.0 MPa
>= 3770 psi
Elongation at Break 550 - 750 %
550 - 750 %
Chemical Properties Metric English Comments
Styrene Content 22.5 - 24.5 %
22.5 - 24.5 %
Descriptive Properties Value Comments
Loss During Drying <0.35%
Mass Share Adigol-2 0.7-1.2%
Mass Share of A-Methyl Styrene 22-25%
Mass Share of P-23 0.4-1.2%
Mass Share of VS-30A 1-2%
Mass Share of VTS-150 1-1.4%
Spread Flow Batch Error <±6 %