Sibur SKI-3S 1st Grade, 1st Group Isoprene Rubber (IR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur SKI-3S 1st Grade, 1st Group Isoprene Rubber (IR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. It is used instead of natural rubber during production of colored rubber articles, medical articles, and rubbers contacting with food products.
Physical Properties Metric English Comments
Mooney Viscosity 72 - 88

@Temperature 100 °C
72 - 88

@Temperature 212 °F
ML 1-4
Ash <= 0.50 %
<= 0.50 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 29.4 MPa
>= 4260 psi
Tensile Strength, Ultimate >= 20.6 MPa

@Temperature 100 °C
>= 2990 psi

@Temperature 212 °F
Descriptive Properties Value Comments
Loss During Drying <1.2%
Mass Share Adigol-2 0.2-0.6%
Mass Share Agidol-1 0.5-1.3%
Mass Share Lavinox 22M-46 0.2-0.6%
Mass Share Ralox-46 0.2-0.6%
Spread Flow Batch Error <±10 %