Sibur H030 GP/1 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur H030 GP/1 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose product, is used in injection molding, extrusion and thermal molding applications.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
GOST 11645
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
50 mm/min; GOST 11262
Elongation at Yield 10 %
10 %
50 mm/min; GOST 11262
Flexural Modulus 1.50 GPa
218 ksi
5 mm/min; GOST 9550
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
GOST 19109
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
GOST 12021
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
GOST 15088
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution