Sibur DST-45 RM Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur DST-45 RM Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kraton D 4271. For production of footwear compositions.
Physical Properties Metric English Comments
Melt Index of Compound 2.0 - 9.0 g/10 min

@Temperature 190 °C
2.0 - 9.0 g/10 min

@Temperature 374 °F
P=49, 1 H
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Tensile Strength at Break >= 11.8 MPa
>= 1710 psi
Elongation at Break >= 930 %
>= 930 %
Chemical Properties Metric English Comments
Styrene Content 43 - 47 %
43 - 47 %
Descriptive Properties Value Comments
Loss During Drying <0.5%