Sibur BK-1675S Butyl Rubber (IIR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur BK-1675S Butyl Rubber (IIR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EXXON Butyl 268, PB 301 Bayer. For use in the construction industry.
Physical Properties Metric English Comments
Mooney Viscosity 35 - 65

@Temperature 100 °C
35 - 65

@Temperature 212 °F
ML 1-4
Descriptive Properties Value Comments
Loss During Drying <0.5%
Spread Flow Batch Error <±8 %
Unsaturation 0.7-2.3%, mol