Material Notes:
With high resistance to burning for bodies of devices, technical articles and consumer goods, and contacting with good products.
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
Melt Index of Compound 7.0 g/10 min
7.0 g/10 min
Mechanical Properties Metric English Comments
Elongation at Break >= 8.0 %
>= 8.0 %
Izod Impact, Notched (ISO) >= 5.00 kJ/m²
>= 2.38 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point <= 95.0 °C
<= 203 °F
Chemical Properties Metric English Comments
Styrene Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Acrylonitrile Content <.001
Impact Tension Strength >5 MPa
Resistance to Burning PB-0