Sibur ABS 2802 Extrusion Grade ABS Plastic

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur ABS 2802 Extrusion Grade ABS Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
With high deformation properties and impact strength for production of sheets with following pneumatic and vacuum forming of products of technical purpose.
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
Melt Index of Compound 1.3 - 2.5 g/10 min
1.3 - 2.5 g/10 min
Mechanical Properties Metric English Comments
Elongation at Break >= 30 %
>= 30 %
Izod Impact, Notched (ISO) >= 34.0 kJ/m²
>= 16.2 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point <= 95.0 °C
<= 203 °F
Descriptive Properties Value Comments
Impact Tension Strength >36.3 MPa