Sibur 140-13P Polyvinyl Chloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur 140-13P Polyvinyl Chloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a period of 20 minutes. For insulation of wires and cables operating in intervals of temperatures from -40°C to 70°C.
Physical Properties Metric English Comments
Density 1.25 - 1.28 g/cc
0.0452 - 0.0462 lb/in³
Water Absorption <= 0.25 %
<= 0.25 %
Collected Volatile Condensable Material <= 2.0 %
<= 2.0 %
Loss in mass at 160°C during 6 hours
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 80
50 - 80
Tensile Strength at Break >= 19.6 MPa
>= 2840 psi
Elongation at Break >= 250 %
>= 250 %
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm

@Temperature 70.0 °C
>= 1.00e+11 ohm-cm

@Temperature 158 °F
>= 5.00e+13 ohm-cm

@Temperature 20.0 °C
>= 5.00e+13 ohm-cm

@Temperature 68.0 °F
Descriptive Properties Value Comments
Color Transparent
Number of Inclusions <24 psc
With dimensions up to 0.5 mm