Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 83.4 MPa
12100 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 4.90 GPa
711 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB
HB