Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Shinkong Synthetic Fibers Corp
Trade Name Shinite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 102 MPa
14800 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Flexural Yield Strength 161 MPa
23300 psi
ASTM D790
Flexural Modulus 8.83 GPa
1280 ksi
ASTM D790
Izod Impact, Notched 0.686 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.29 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 4.0
4.0
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149