Shin-Etsu Silicones X-22-6711D Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones X-22-6711D Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Viscosity Measurement 3000
3000
cs
Optical Properties Metric English Comments
Refractive Index 1.401
1.401
Descriptive Properties Value Comments
Active (%) 25
Appearance Liquid
Diluent (%) 6cs
INCI PEG/PPG-18/18 Dimethicone (and) Isododecane (Tentative)