Material Notes:
SV13500U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product Features: This product can be blended with other ShinEtsu general purpose or no post cure bases for intermediate properties. The choice between these bases will depend on specific requirements. This product can also be extended with extending fillers.Typical Applications: Roll covers.Diaphragms.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
Tensile Strength at Break 10.3 MPa
1500 psi
Elongation at Break 890 %
890 %
100% Modulus 0.000614 GPa
0.0890 ksi
Tear Strength 26.3 kN/m
150 pli
Die B
Compression Set 24 %

@Temperature 177 °C,
Time 79200 sec
24 %

@Temperature 351 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Press Cure