Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones LIMSâ„¢ KE2095-40AB Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name LIMS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones LIMSâ„¢ KE2095-40AB Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KE-2095-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesSelective self adhesionNon adhesion to metalsInsert-molding and co-injection molding availableInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Viscosity 590000 cP
590000 cP
A
970000 cP
970000 cP
B
Linear Mold Shrinkage 0.027 cm/cm
0.027 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength 8.10 MPa
1170 psi
Elongation at Yield 480 %
480 %
Tear Strength 29.0 kN/m
165 pli
Compression Set 6.0 %

@Temperature 200 °C,
Time 14400 sec
6.0 %

@Temperature 392 °F,
Time 4.00 hour
25 %

@Temperature 150 °C,
Time 3600 sec
25 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
Press Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 26
T10 (302°F, ODR)
42
T90 (302°F, ODR)
Regulatory Testing Class VI