Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
True
Bulk Density 0.400 g/cc
0.0145 lb/in³
Apparent
Volatiles 0.10 %
0.10 %
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Rubber
Optical Properties Metric English Comments
Refractive Index 1.41
1.41
Descriptive Properties Value Comments
Glyceryl Trioctanoate 4
INCI Vinyl Dimethicone/Methicone Silsesquioxane Crosspolymer
Isononyl Isonononoate 8
Iso-parafin 4
Nature of Silicone Rubber Core Dimethyl
Shape Sphere
Squalane 6
no swell
Swell (g/5g) 15
6cs
19
D5
Users viewing this material also viewed the following: