Shin-Etsu Silicones KF-7002 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KF-7002 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
Descriptive Properties Value Comments
Active (%) 100
Appearance Wax
INCI Stearoxymethicone/Dimethicone Copolymer
M.P. 40-50
Nature of Silicone Rubber Core Stearoxy modified
VM 1