Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ShinEtsu KEG200170 is a very fast cure liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KEG200170 is low enough to allow easy pumping through most injection molding systems.Product Features: High tear strengthRapid cure time at elevated temperature Long pot life at room temperatureTypical Applications: O-rings.Diaphragms.Capping.Rubber rollers.Connector packings.Other electrical parts.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength at Break 10.2 MPa
1480 psi
Elongation at Break 564 %
564 %
Tear Strength 39.1 kN/m
223 pli
Die B
Compression Set 9.0 %

@Temperature 180 °C,
Time 79200 sec
9.0 %

@Temperature 356 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Type Press Cure/Post Cure