Shin-Etsu Silicones KE-7022U Temperature Resistant Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-7022U Temperature Resistant Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KE7022 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 300 °C(67 ~ +570 °F).Typical Applications: PPC Rollers.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength at Break 7.72 MPa
1120 psi
Elongation at Break 275 %
275 %
Tear Strength 11.4 kN/m
65.0 pli
Die B
Compression Set 7.0 %

@Temperature 180 °C,
Time 79200 sec
7.0 %

@Temperature 356 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Post Cure