Material Notes:
ShinEtsu FEA251 U is one of a series of fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series for intermediate hardnesses.Product Features: Excellent fuel and solvent resistance..Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
Tensile Strength at Break 9.79 MPa
1420 psi
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Post Cure