Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermoplastic. This grade combines high melt strength and viscosity with high chemical resistance and barrier performance. Moreover, this material exhibits a high impact resistance, both at room temperature and at lower temperatures, and good creep performance. CARILON Polymer D26CX100 can also withstand short-term exposure to elevated temperatures. CARILON Polymer D26CX100 has been designed for demanding extrusion processes. This grade should be considered for liners, pipes and large blow moldings.Data provided by Shell Chemical.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Water Absorption 0.45 %
0.45 %
24 hour immersion; ASTM D570
Moisture Absorption at Equilibrium 0.53 %
0.53 %
at 50% RH at Equilibrium; ASTM D570
Water Absorption at Saturation 2.1 %
2.1 %
at saturation; ASTM D570
Melt Flow 2.7 g/10 min

@Load 2.16 kg,
Temperature 240 °C
2.7 g/10 min

@Load 4.76 lb,
Temperature 464 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 63.0 MPa
9140 psi
ASTM D638
Tensile Strength, Yield 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Elongation at Yield 25 %
25 %
ASTM D638
Tensile Modulus 1.60 GPa
232 ksi
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 210 °C
410 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 240 °C
464 °F
At Die
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved