Material Notes:
Special Properties: Hot abrasion, Wear resistanceIndustry: SteelApplication: False Chute, Tundish BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.75 g/cc
>= 0.0994 lb/in³
After Drying at 110°C
Grain Size <= 10000 µm
<= 10000 µm
Mechanical Properties Metric English Comments
Compressive Strength 98.1 MPa

@Temperature 110 °C
14200 psi

@Temperature 230 °F
Cold Crushing
118 MPa

@Temperature 1100 °C
17100 psi

@Temperature 2010 °F
Cold Crushing
127 MPa

@Temperature 1500 °C
18500 psi

@Temperature 2730 °F
Cold Crushing
39.2 MPa

@Time 86400 sec
5690 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1700 °C
3090 °F
Descriptive Properties Value Comments
Refractoriness >1820°C
Thermal Expansion 0.65
Reversible
Water Required to Mix 10-12%