Sharadaa Ceramics REFINSUL ZAP-019 Insulating Castables

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics REFINSUL ZAP-019 Insulating Castables.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for low density and low thermal conductivity, and are helpful in conserving heat energy thus reducing fuel costs.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density <= 1.45 g/cc
<= 0.0524 lb/in³
Dried at 110°C
Mechanical Properties Metric English Comments
Modulus of Rupture 0.001765 GPa
0.2560 ksi
Dried at 110°C
0.00137 GPa

@Treatment Temp. 800 °C
0.199 ksi

@Treatment Temp. 1470 °F
0.00147 GPa

@Treatment Temp. 1300 °C
0.213 ksi

@Treatment Temp. 2370 °F
Compressive Strength 3.92 MPa
569 psi
Fired at 800°C, Cold Crushing
4.90 MPa
711 psi
Fired at Service temp. of 1300°C, Cold Crushing
8.34 MPa
1210 psi
Dried at 110°C, Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity <= 0.465 W/m-K

@Temperature 500 °C
<= 3.23 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Al2O3 >= 42 %
>= 42 %
Fe2O3 <= 1.5 %
<= 1.5 %
Descriptive Properties Value Comments
Permanent Linear Change -0.2 - 0.2%
Fired at 800°C
-0.6 - 0.6%
Fired at Service temp. 1300°C