Shanghai Ofluorine D-1 PVDF Lithium Ion Battery Binders (DF-2)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Shanghai Ofluorine
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shanghai Ofluorine D-1 PVDF Lithium Ion Battery Binders (DF-2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: D-1 PVDF Powder has good solubility in some solvent, it is more suitable for lithium ion battery industry as binder. D-1 PVDF is a homopolymer with high dielectric constant, which shows high viscosity and bonding properties in some solvent, easy to form film. D-1 PVDF powder as raw materials, the lithium ion battery membrane have good chemical stability, temperature stability, excellent mechanical strength and processability.Information provided by Shanghai Ofluorine Chemical Technology
Physical Properties Metric English Comments
Specific Gravity 1.74 - 1.77 g/cc
1.74 - 1.77 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
Karl Fischer
Viscosity Measurement 1.0 - 2.0

@Temperature 30.0 °C
1.0 - 2.0

@Temperature 86.0 °F
[dL/g] DMA, Intrinsic Viscosity
>= 200

@Temperature 30.0 °C
>= 200

@Temperature 86.0 °F
[mPa.S] 1g/ml MNP, Rotary Viscosity
Thermal Properties Metric English Comments
Melting Point 158 - 168 °C
316 - 334 °F
ASTM D3418
Descriptive Properties Value Comments
Appearance White solid powder
Purity 0.995
Solubility no impurity and insoluble matter
1g/10ml NMP
Solution is clear and transparent
30°C, 1hr