Shandong Guangyin GYBHVNP Polymer

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Shandong Guangyin
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Guangyin GYBHVNP Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Our GYBHVNP products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 50.0 MPa
>= 7250 psi
ISO 3146
Elongation at Break >= 300 %
>= 300 %
ISO 527
Flexural Strength >= 10.0 MPa
>= 1450 psi
ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 179/IeU
Izod Impact, Unnotched (ISO) NB
NB
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 189 - 192 °C
372 - 378 °F
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %