Shakespeare WN-20 diameter 0.2 mm Nylon 66 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WN-20 diameter 0.2 mm Nylon 66 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentAbrasion resistantNylon 6,6Low modulusWeft yarnLow shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 45 %
45 %
Elongation at Yield 10 %
10 %
at 3 g/D
Thermal Properties Metric English Comments
Shrinkage 4.00 %

@Temperature 200 °C
4.00 %

@Temperature 392 °F