Shakespeare SPX-501 diameter 0.5 mm Polyetherketone Monofilament

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare SPX-501 diameter 0.5 mm Polyetherketone Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentPEEKHigh Temperature ApplicationsHigh modulusMedium shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 26 %
26 %
Elongation at Yield 3.0 %
3.0 %
at 1.75 g/D
Thermal Properties Metric English Comments
Shrinkage 8.50 %

@Temperature 200 °C
8.50 %

@Temperature 392 °F