Shakespeare NX-315 diameter 0.13 mm Nylon 66 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare NX-315 diameter 0.13 mm Nylon 66 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentNylon 6,6Moderate ModulusMedium shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 27 %
27 %
Elongation at Yield 3.5 %
3.5 %
at 1.75 g/D
Thermal Properties Metric English Comments
Shrinkage 12.0 %

@Temperature 177 °C
12.0 %

@Temperature 351 °F