Shakespeare NX-122 diameter 0.2 mm Nylon Monofilament 610

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare NX-122 diameter 0.2 mm Nylon Monofilament 610.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10Low modulusLow moisture regainLow shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 50 %
50 %
Elongation at Yield 12 %
12 %
at 1.75 g/D
Thermal Properties Metric English Comments
Shrinkage 2.00 %

@Temperature 175 °C
2.00 %

@Temperature 347 °F