Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Shakespeare Company
Trade Name Isocor™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isocorâ„¢ 653 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ 653 is easily processed and has a wide range of applications due to its physical properties, chemical resistance, and lower melt temperatures. Used for film extrusion, pigment carriers, and specialty adhesives.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D 792
Water Absorption 3.5 %
3.5 %
24 hour immersion; ASTM D 570
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
ASTM D 2240
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D 638
Elongation at Break >= 350 %
>= 350 %
ASTM D 638
Flexural Modulus 0.621 GPa
90.0 ksi
ASTM D 790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D 256
0.427 J/cm

@Temperature -40.0 °C
0.800 ft-lb/in

@Temperature -40.0 °F
ASTM D 648
Users viewing this material also viewed the following: